2Cr13 Stainless Steel Introduction

Chinese 2Cr13 steel (20Cr13) is a martensitic stainless steel with magnetic properties, good corrosion resistance and high hardness in the quenched state.

 

2Cr13 stainless steel is used in a wide range of applications, such as cutting tools, surgical tools, and steam turbine blades, material density is 7.75g/cm3, 2Cr13 is an old representation, the new representation is 20Cr13.

 

Steel Grade Designation Of 20Cr13 = 2Cr13 Stainless Steel

20 (or 2) – Average carbon content: 20/10,000 (0.2%), old designation is 2/1,000

Cr – Chromium symbol

13 – Average content of chromium: 13%

 

2Cr13 Material Equivalent

China   USA   Germany   Japan  
Standard Grade Standard Grade (UNS) Standard Grade Standard Grade
GB/T 1220; 20Cr13 AISI, 420 DIN EN 10088-2; X20Cr13 (1.4021) JIS G4303 SUS 420J1

 

Chemical Composition Of (20Cr13) 2Cr13 Stainless Steel

C Si (≤) Mn (≤) P (≤) S (≤) Cr Ni (≤)
0.16 – 0.25 1 1 0.04 0.03 12.00 – 14.00 -0.6

 

(20Cr13) 2Cr13 Steel Mechanical Properties

For Hot Rolled Steel Bar After Quenching and Tempering

Tensile strength: 640 N/mm2

Conditional yield strength (Non-proportional extension strength): ≥440 N/mm2

Elongation: ≥20%

Rate of reduction in area: ≥50%

Impact energy: ≥63 Aku2 (J)

Material hardness:

HBW: ≤ 223 (After annealing);

HBW: ≥ 192 (After quenching and tempering)

Notes:

Data is for steel diameter (d) less than or equal to 75mm.

1 N/mm2 = 1 MPa

 

Physical Properties

Density (g/cm3): 7.75

Melting point: 1470-1510℃

Specific heat capacity (J/Kg·K): 460 at 0-100℃

Thermal conductivity (W/m·K):

22.2 at 100℃

26.4 at 500℃

Coefficients of linear thermal expansion (10-6/K):

10.3 (0-100℃)

12.2 (0-500℃)

Electrical Resistivity (μΩ·m): 0.55 at 20℃

Longitudinal modulus of elasticity (kN/mm2): 200 at 20℃

 

Heat Treatment

Annealing: 800-900℃ (Slow cooling)

Quenching: 920-980℃ (Cooling: Oil)

Tempering: (600-750℃) (Rapid cooling)

 